How to fix poor bed adhesion or warping?

3d-printer-7.png3d-printer-8.png

Layers bulging outward or downward, poor adhesion, or warping are typically caused by overheating.

1. Print temperature too high: Refer to Section 3.1.2 Advanced Printing to reduce the nozzle temperature.

2. Printing speed too high: Refer to Section 3.1.2 Advanced Printing to reduce print speed. In Standard mode, the default is 300 mm/s — try reducing by 10–20 mm/s and observe.